항산화제 168 Supplier for Polymer Processing

SUNNOX® 168 is a hydrolysis-resistant phosphite secondary antioxidant. Blended with a phenolic primary such as 1010 또는 1076, it protects color and melt flow while polyolefins and engineering plastics are extruded and molded.

CAS 31570-04-4 · Phosphite · Secondary antioxidant
Illustration of polymer pellets, molded samples and film
Polymer application illustration — not a photograph of the product

제품개요

항산화제 168 decomposes the hydroperoxides that form when polymer melts are sheared and heated, so it stops the chain reaction that causes yellowing, gels and melt-flow drift during processing. It is rarely used alone: the standard approach is a blend with a phenolic primary antioxidant, which carries the long-term protection in service. 168:1010 ~에 1:1 또는 2:1 is the most common starting blend in PP and PE.

Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.

Key Benefits

Color and melt-flow protection

Keeps yellowness index and MFR stable through extrusion, molding and regrind, where most processing damage happens.

Works with your phenolic

Synergistic with 1010 그리고 1076. Adding 168 often lets you hold or reduce the phenolic level for the same processing stability.

Hydrolysis resistant

More tolerant of humid storage and long sea transit than many other phosphites, so the powder stays free-flowing and active.

기술 사양

Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.

매개변수Typical value
제품명항산화제 168
상표SUNNOX® 168
CAS 번호.31570-04-4
화학명트리스(2,4-디-tert-부틸페닐) 인화물
분자식C42H63O3P
분자 무게646.9
모습백색 결정 분말
시험≥99.0%
녹는 점183–187 °C
Volatile Matter≤0.5% (105 ℃, 2 시간)
Light Transmittance — 425 nm≥98%
Light Transmittance — 500 nm≥98%

Applications by Polymer

Pick a material family to see how 168 is normally used and what to confirm before your trial.

Illustration of polymer film, molded components and masterbatch granules
Polymer application illustration

Polyolefins — PE & PP

The largest use of 168. Typical packages: 168:1010 1:1 또는 2:1 for PP injection and fiber, 168:1076 for film. Total package levels of about 0.1–0.3% in PP and 0.05–0.15% in PE film are common starting points.

What to confirm for your application

  • Resin grade, catalyst type and MFR target
  • Number of extrusion passes and regrind share
  • Current antioxidant package and dosage
Discuss this application →

Polyamide — PA

Used with a phenolic primary to limit discoloration during compounding of PA6 and PA66, including glass-filled grades.

What to confirm for your application

  • PA type and filler content
  • Processing temperature and residence time
  • Color target (YI or ΔE) after molding
Discuss this application →

Polycarbonate — PC

Helps protect clarity and color at the high melt temperatures PC needs. Usually dosed low, alongside the base resin stabilizer.

What to confirm for your application

  • PC grade and whether it is a blend (PC/ABS)
  • Melt temperature and optical requirements
  • Existing stabilizer system
Discuss this application →

ABS & Styrenics

Added with a phenolic antioxidant to reduce yellowing and property loss during compounding and molding of ABS and HIPS.

What to confirm for your application

  • ABS / HIPS grade and other additives
  • Heat history in compounding and molding
  • Color and impact retention targets
Discuss this application →

포장 & 저장

포장

25 kg net bags or cartons. Pallet wrapping and private-label bags on request.

저장

Keep sealed in a cool, dry place away from heat and moisture. See the SDS for full handling details.

리드타임 & terms

Typically 3–15 business days from order confirmation, depending on quantity. 본선 인도, CIF or DAP to major ports.

인위적인 & Buying Information

Selecting an Antioxidant System

Your requirementWhat usually works
Color and melt-flow stability during extrusion or moldingPhosphite secondary antioxidant (168) with a phenolic primary
Long-term heat aging in serviceHigh-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP)
Thin film, 섬유, low-melting compoundingLower-melting phenolic (1076) for easy dispersion
Repeated processing / 재활용 콘텐츠Raise the phosphite share in the blend and check yellowing after each pass
Humid storage or long transitHydrolysis-resistant phosphite such as 168; keep bags sealed
Food-contact articlesAsk for the grade-specific food-contact statement before trials
Replacing an existing gradeSend your current TDS or COA; we match on the parameters you approve

Antioxidant Comparison

Swipe or scroll horizontally to see all columns →

제품유형Mol. weight녹는 점Main jobTypical starting level*
SUNNOX® 168Phosphite · secondary646.9183–187 °C가공 안정성, 색상0.05–0.2% with a phenolic
SUNNOX® 1010Hindered phenol · primary1177.6110–125°CLong-term thermal protection0.05–0.3%
SUNNOX® 1076Hindered phenol · primary530.950–55 °CLong-term protection, easy dispersion0.05–0.3%
SUNNOX® DLTDPThioester · secondary514.838-42°CHeat-aging synergist0.1–0.3% with a phenolic
SUNNOX® DSTDPThioester · secondary683.263–69 °CHeat-aging synergist, 낮은 변동성0.1–0.3% with a phenolic

*Starting points for trials, not fixed recommendations. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.

서류 & 품질

COA — 분석 증명서

Issued for every batch shipped, with the test results for that lot.

TDS — 기술 데이터 시트

Typical properties and specification for evaluation and supplier approval.

SDS — Safety Data Sheet

GHS-format handling, storage and transport information.

샘플

Lab samples for evaluation; tell us the test you plan to run so the sample size fits.

Third-party testing

SGS or Intertek testing can be arranged on request.

Regulatory statements

도달하다, food-contact and other statements are issued per grade and destination; ask before ordering.

항산화제 168 구매자 가이드

Name the failure you want to prevent

Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.

Start from a proven blend

Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.

Compare the numbers that matter

For powders: 시험, melting range, volatiles and light transmittance at 425/500 nm (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.

Lock in supply terms

Agree packaging, monthly volume, destination port and required documents up front. A matching CAS number alone does not qualify a new source; run your trial and keep the approved lot COA as the reference.

Request a Quotation for Antioxidant 168

Start with your polymer, 수량 및 목적지. Add your current grade or specification and we will quote against it.

InformationExample
중합체 / MaterialPP, 체육, ABS, 화합물, 마스터배치
애플리케이션Injection molding, 압출, 영화, 섬유
Current additiveGrade or supplier you use today
Required specificationYour TDS, COA or key limits
QuantityTrial order / monthly / annual volume
포장Standard 25 kg or specific requirement
DestinationCountry and port
Documents neededCOA, SDS, 도달하다, food-contact statement
Send RFQ by EmailContact SUNCHEM →

Related Antioxidants

SUNNOX® 1010

High-MW hindered phenolic primary antioxidant for long-term thermal protection with low volatility.

View product →

SUNNOX® 1076

Low-melting hindered phenolic primary antioxidant, easy to disperse in film and compounding.

View product →

SUNNOX® DLTDP

Thioester secondary antioxidant that boosts long-term heat aging when used with a phenolic.

View product →

SUNNOX® DSTDP

Higher-melting thioester synergist with lower volatility for long-term heat aging.

View product →

항산화제 168 자주하는 질문

What ratio of 168 에게 1010 should I start with?

1:1 그리고 2:1 (168:1010) are the most widely used starting blends in polyolefins. Use 2:1 when processing stability and color are the main concern, 1:1 when long-term heat aging matters as much. Confirm the ratio in your own trial.

항산화제 가능 168 be used alone?

It can, but it is not recommended. 168 protects during processing; it does little for long-term aging in service. Pair it with a phenolic primary antioxidant such as 1010 또는 1076.

Which COA parameters should I check on incoming lots?

시험, melting range, volatiles and light transmittance at 425 그리고 500 nm. Transmittance is the quickest indicator of color quality in the final part.

Can I get a sample before ordering?

예. Tell us the polymer, the test you plan to run and the quantity you need. Samples ship with a COA so you can compare the lot against your current material.

What if a COA does not match our agreed specification?

Send us the agreed specification and the COA showing the difference (parameter, unit and test method). We check it with the production batch record before you accept the material, and replace or re-test where the lot is out of specification.

Discuss Your Antioxidant 168 Requirements

Send your application, specification and quantity to request a quotation or supporting documents.

돋보기