Long-term heat protection
Keeps tensile and impact properties through long service at elevated temperature, the main reason 1010 is the default phenolic in polyolefins.
SUNNOX® 1010 is a high-molecular-weight hindered phenolic primary antioxidant. It gives long-term thermal protection with very low volatility and extraction, in polyolefins, 엔지니어링 플라스틱, rubber and adhesives.
항산화제 1010 traps the free radicals that drive thermal oxidation, so plastics keep their strength and appearance through years of service at elevated temperature. Its molecular weight of 1177.6 keeps it in the polymer: it does not evaporate during processing and resists extraction by water and solvents. For processing stability it is normally blended with a phosphite such as 168, and with a thioester (DLTDP / DSTDP) where long-term heat aging is critical.
Keeps tensile and impact properties through long service at elevated temperature, the main reason 1010 is the default phenolic in polyolefins.
High molecular weight means low volatility in processing and low migration or extraction in use.
Used in PE, PP, 포엠, ABS, 추신, PVC, 아빠, 애완 동물, PU, 고무, hot-melt adhesives and lubricants. Odorless and non-staining.
| 매개변수 | 일반적인 값 |
|---|---|
| 제품명 | 항산화제 1010 |
| 상표 | SUNNOX® 1010 |
| CAS 번호. | 6683-19-8 |
| 화학명 | 펜타에리트리톨 테트라키스[3-(3,5-디-tert-부틸-4-히드록시페닐)propionate] |
| 분자식 | C73H108O12 |
| 분자 무게 | 1177.6 |
| 모습 | 백색 결정 분말 |
| 녹는 점 | 110–125°C |
| Effective Content | ≥98.0% |
| Main Component | ≥94.0% |
| 금연 건강 증진 협회 | 0.1% 이하 |
| 휘발성 물질 | 0.5% 이하 |
| Light Transmittance — 425 nm | ≥96% |
| Light Transmittance — 500 nm | ≥98% |
| 용해도 (20 ℃, 승/승) | Chloroform 71%, 디클로로메탄 63%, 벤젠 55%, 에틸 아세테이트 47%, 아세톤 46%, 메탄올 0.9%, hexane 0.3%, 물 <0.01% |
일반적인 사양. 모든 배송에는 배치 COA가 함께 제공됩니다.; 귀하의 주문에 적용되는 한도는 견적 및 계약서에서 확인됩니다..
Pick a material family to see how 1010 일반적으로 사용되는 것과 평가판 전에 확인해야 할 사항.
The default long-term antioxidant for PP and PE pipe, 영화, fiber and molded parts. Typically 0.05–0.3%, blended with 168 (1:1 또는 1:2 1010:168) for processing stability.
Used for heat-aging protection in POM, 아빠, PET/PBT, ABS and PS, often at the higher end of the dosage range for parts exposed to heat.
Protects SBS, SIS, EPDM and EVA-based hot-melts and adhesives from oxidation during melting and storage, without staining.
Used as a co-antioxidant in PVC and PU systems and as a high-temperature antioxidant in lubricants and oils.
| 귀하의 요구 사항 | 일반적으로 작동하는 것 |
|---|---|
| Color and melt-flow stability during extrusion or molding | Phosphite secondary antioxidant (168) with a phenolic primary |
| Long-term heat aging in service | High-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP) |
| Thin film, 섬유, low-melting compounding | Lower-melting phenolic (1076) for easy dispersion |
| Repeated processing / 재활용 콘텐츠 | Raise the phosphite share in the blend and check yellowing after each pass |
| Humid storage or long transit | Hydrolysis-resistant phosphite such as 168; keep bags sealed |
| Food-contact articles | Ask for the grade-specific food-contact statement before trials |
| 기존 등급 대체 | 현재 TDS 또는 COA 보내기; 우리는 귀하가 승인한 매개변수와 일치합니다 |
모든 열을 보려면 가로로 스와이프하거나 스크롤하세요 →
| 제품 | 유형 | 몰. 무게 | 녹는 점 | Main job | 일반적인 시작 레벨* |
|---|---|---|---|---|---|
| SUNNOX® 1010 | Hindered phenol · primary | 1177.6 | 110–125°C | Long-term thermal protection | 0.05–0.3% |
| SUNNOX® 168 | Phosphite · secondary | 646.9 | 183–187 °C | 가공 안정성, 색상 | 0.05–0.2% with a phenolic |
| SUNNOX® 1076 | Hindered phenol · primary | 530.9 | 50–55 °C | Long-term protection, easy dispersion | 0.05–0.3% |
| SUNNOX® DLTDP | Thioester · secondary | 514.8 | 38-42°C | Heat-aging synergist | 0.1–0.3% with a phenolic |
| SUNNOX® DSTDP | Thioester · secondary | 683.2 | 63–69 °C | Heat-aging synergist, 낮은 변동성 | 0.1–0.3% with a phenolic |
*시험의 출발점, 고정되지 않은 추천. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.
25 kg net in a plastic inner bag inside a paperboard drum or carton. Private-label packing on request.
Stable under normal conditions. Keep sealed, away from heat and moisture. 전체 취급 세부정보는 SDS를 참조하세요..
일반적으로 주문 확인 후 영업일 기준 3~15일, 수량에 따라. 본선 인도, 주요 포트에 대한 CIF 또는 DAP.
Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.
Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.
For powders: 시험, melting range, volatiles and light transmittance at 425/500 nm (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.
Agree packaging, monthly volume, destination port and required documents up front. 일치하는 CAS 번호만으로는 새로운 출처에 적합하지 않습니다.; run your trial and keep the approved lot COA as the reference.
Start with your polymer, 수량 및 목적지. Add your current grade or specification and we will quote against it.
| 정보 | 예 |
|---|---|
| 중합체 / 재료 | PP, 체육, ABS, 화합물, 마스터배치 |
| 애플리케이션 | 사출 성형, 압출, 영화, 섬유 |
| 현재 첨가제 | 현재 사용하는 등급 또는 공급업체 |
| 필수사양 | 귀하의 TDS, COA 또는 키 제한 |
| 수량 | 평가판 주문 / 월간 간행물 / 연간 볼륨 |
| 포장 | 기준 25 kg 또는 특정 요구 사항 |
| 목적지 | 국가 및 항구 |
| 필요한 서류 | COA, SDS, 도달하다, 식품 접촉 진술서 |
Hydrolysis-resistant phosphite secondary antioxidant for color and melt-flow protection during processing.
상품보기 →Low-melting hindered phenolic primary antioxidant, easy to disperse in film and compounding.
상품보기 →Thioester secondary antioxidant that boosts long-term heat aging when used with a phenolic.
상품보기 →Higher-melting thioester synergist with lower volatility for long-term heat aging.
상품보기 →Both are hindered phenolic primaries. 1010 (MW 1177.6) has lower volatility and extraction, so it is preferred for long service life and high-temperature use. 1076 (MW 530.9, melts at 50–55 °C) disperses more easily in film and low-temperature compounding.
0.05–0.3% in most polyolefins, higher for parts that must pass long heat-aging tests. Use it with 168 for processing stability. Confirm the level in your own heat-aging trial.
1010 is widely used in food-contact polymers. Ask us for the grade-specific food-contact statement for your market before you start trials.
예. 폴리머를 알려주세요, 실행하려는 테스트와 필요한 수량. 샘플은 COA와 함께 배송되므로 현재 자재와 로트를 비교할 수 있습니다..
합의된 사양과 차이점을 보여주는 COA를 보내주세요. (매개변수, 단위 및 시험방법). 자재를 승인하기 전에 생산 배치 기록을 통해 확인합니다., 로트가 사양을 벗어난 경우 교체하거나 다시 테스트합니다..