Easy dispersion
Melts at 50–55 °C, so it mixes evenly in film, fiber and low-temperature compounding.
SUNNOX® 1076 is a non-staining hindered phenolic primary antioxidant. Its low melting point makes it easy to disperse in film, fiber and low-temperature compounding, where it gives long-term thermal protection.
항산화제 1076 scavenges the free radicals that drive thermal oxidation in plastics, 엘라스토머 및 접착제. Compared with 1010 it has a lower molecular weight (530.9) and melts at 50–55 °C, so it blends readily into polyolefin film, PVC and hot-melts. It is normally combined with a phosphite such as 168 for processing stability, and with a thioester such as DLTDP for long-term heat aging.
Melts at 50–55 °C, so it mixes evenly in film, fiber and low-temperature compounding.
Good color and low odor in finished parts, with resistance to water extraction.
Pairs with phosphites for processing stability and with thioesters for long-term heat aging.
| 매개변수 | 일반적인 값 |
|---|---|
| 제품명 | 항산화제 1076 |
| 상표 | SUNNOX® 1076 |
| CAS 번호. | 2082-79-3 |
| 화학명 | Octadecyl 3-(3,5-디-tert-부틸-4-히드록시페닐)propionate |
| 분자식 | C35H62O3 |
| 분자 무게 | 530.9 |
| 모습 | 백색 결정 분말 |
| 녹는 점 | 50–55 °C |
| 콘텐츠 | ≥98.0% |
| 휘발성 물질 | ≤0.2% |
| 금연 건강 증진 협회 | 0.1% 이하 |
| Light Transmittance — 425 nm | ≥97% |
| Light Transmittance — 500 nm | ≥98% |
일반적인 사양. 모든 배송에는 배치 COA가 함께 제공됩니다.; 귀하의 주문에 적용되는 한도는 견적 및 계약서에서 확인됩니다..
방법을 보려면 애플리케이션을 선택하세요. 1076 일반적으로 사용되는 것과 평가판 전에 확인해야 할 사항.
The main use of 1076. Typically 0.05–0.3%, often as 168:1076 blends for film where easy dispersion matters.
Used as a co-antioxidant in PVC and styrenic compounds to limit heat yellowing during processing.
Protects EVA, SBS and polyolefin hot-melts and elastomers from oxidation in the melt tank and in service.
| 귀하의 요구 사항 | 일반적으로 작동하는 것 |
|---|---|
| Color and melt-flow stability during extrusion or molding | Phosphite secondary antioxidant (168) with a phenolic primary |
| Long-term heat aging in service | High-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP) |
| Thin film, 섬유, low-melting compounding | Lower-melting phenolic (1076) for easy dispersion |
| Repeated processing / 재활용 콘텐츠 | Raise the phosphite share in the blend and check yellowing after each pass |
| Humid storage or long transit | Hydrolysis-resistant phosphite such as 168; keep bags sealed |
| Food-contact articles | Ask for the grade-specific food-contact statement before trials |
| 기존 등급 대체 | 현재 TDS 또는 COA 보내기; 우리는 귀하가 승인한 매개변수와 일치합니다 |
모든 열을 보려면 가로로 스와이프하거나 스크롤하세요 →
| 제품 | 유형 | 몰. 무게 | 녹는 점 | Main job | 일반적인 시작 레벨* |
|---|---|---|---|---|---|
| SUNNOX® 1076 | Hindered phenol · primary | 530.9 | 50–55 °C | Long-term protection, easy dispersion | 0.05–0.3% |
| SUNNOX® 1010 | Hindered phenol · primary | 1177.6 | 110–125°C | Long-term thermal protection | 0.05–0.3% |
| SUNNOX® 168 | Phosphite · secondary | 646.9 | 183–187 °C | 가공 안정성, 색상 | 0.05–0.2% with a phenolic |
| SUNNOX® DLTDP | Thioester · secondary | 514.8 | 38-42°C | Heat-aging synergist | 0.1–0.3% with a phenolic |
| SUNNOX® 245 | Hindered phenol · primary | 586.8 | 76–79 °C | Styrenics, 포엠, 아빠, PU | 0.1–0.3% |
*시험의 출발점, 고정되지 않은 추천. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.
25 PE 내부 라이너가 있는 kg 순백 또는 상자. 팔레트화; 요청 시 개인 라벨 포장.
밀봉하여 서늘한 곳에 보관하세요, 마른, 열과 직사광선을 피해 통풍이 잘되는 곳. 전체 취급 세부정보는 SDS를 참조하세요..
일반적으로 주문 확인 후 영업일 기준 3~15일, 수량에 따라. 본선 인도, 주요 포트에 대한 CIF 또는 DAP.
Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.
Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.
For powders: 시험, melting range, volatiles and light transmittance at 425/500 nm (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.
Agree packaging, monthly volume, destination port and required documents up front. 일치하는 CAS 번호만으로는 새로운 출처에 적합하지 않습니다.; run your trial and keep the approved lot COA as the reference.
Start with your polymer, 수량 및 목적지. Add your current grade or specification and we will quote against it.
| 정보 | 예 |
|---|---|
| 중합체 / 재료 | PP, 체육, ABS, 화합물, 마스터배치 |
| 애플리케이션 | 사출 성형, 압출, 영화, 섬유 |
| 현재 첨가제 | 현재 사용하는 등급 또는 공급업체 |
| 필수사양 | 귀하의 TDS, COA 또는 키 제한 |
| 수량 | 평가판 주문 / 월간 간행물 / 연간 볼륨 |
| 포장 | 기준 25 kg 또는 특정 요구 사항 |
| 목적지 | 국가 및 항구 |
| 필요한 서류 | COA, SDS, 도달하다, 식품 접촉 진술서 |
High-MW hindered phenolic primary antioxidant for long-term thermal protection with low volatility.
상품보기 →Hydrolysis-resistant phosphite secondary antioxidant for color and melt-flow protection during processing.
상품보기 →Thioester secondary antioxidant that boosts long-term heat aging when used with a phenolic.
상품보기 →Choose 1076 when easy dispersion and low-temperature processing matter (영화, PVC, hot-melts). Choose 1010 when you need the lowest volatility and extraction for long service at high temperature.
0.05–0.3% in most polyolefins, usually with 168 for processing stability. Confirm the level in your own trial.
예, it is widely used in food-contact polymers. Ask us for the grade-specific food-contact statement for your market.
예. 폴리머를 알려주세요, 실행하려는 테스트와 필요한 수량. 샘플은 COA와 함께 배송되므로 현재 자재와 로트를 비교할 수 있습니다..
합의된 사양과 차이점을 보여주는 COA를 보내주세요. (매개변수, 단위 및 시험방법). 자재를 승인하기 전에 생산 배치 기록을 통해 확인합니다., 로트가 사양을 벗어난 경우 교체하거나 다시 테스트합니다..