CAS 번호.123-28-4
유형Thioester · Secondary
모습White crystalline powder or flake
녹는 점38-42°C
산가≤0.05 mg KOH/g

제품개요 & 주요 이점

DLTDP decomposes hydroperoxides into stable products, so it removes the fuel for continued oxidation during long service at elevated temperature. On its own it is a weak antioxidant; combined with a hindered phenol it gives a strong synergy for heat-aging performance. Typical blends run at 1:1 에게 1:3 페놀성:DLTDP.

Long-term heat aging

Synergy with phenolic antioxidants extends oven-aging life well beyond the phenolic alone.

Low melting point

Melts at 38–42 °C and disperses easily in compounding and masterbatch.

Cost-effective boost

Often lets you hold or reduce the phenolic level for the same heat-aging target.

기술 사양

매개변수일반적인 값
제품명항산화제 DLTDP
상표SUNNOX® DLTDP
CAS 번호.123-28-4
화학명Dilauryl 3,3'-thiodipropionate
분자식C30H58O4S
분자 무게514.8
모습White crystalline powder or flake
녹는 점38-42°C
Acid Value≤0.05 mg KOH/g
휘발성 물질≤0.05%

일반적인 사양. 모든 배송에는 배치 COA가 함께 제공됩니다.; 귀하의 주문에 적용되는 한도는 견적 및 계약서에서 확인됩니다..

폴리머별 응용

Pick an application to see how DLTDP is normally used and what to confirm before your trial.

폴리올레핀

Used with 1010 또는 1076 in PP and PE parts that must pass long oven-aging tests, such as appliance and automotive components.

시험 전 확인

  • Heat-aging test (온도, 시간)
  • Phenolic antioxidant and its level
  • Odor requirements for the part
이 애플리케이션에 대해 토론 →

고무, 접착제 & 윤활유

Used in rubber, hot-melts and lubricants as a heat-aging synergist.

시험 전 확인

  • Base polymer or oil
  • Operating temperature
  • Existing antioxidant package
이 애플리케이션에 대해 토론 →

선택 & 비교

Selecting an Antioxidant System

귀하의 요구 사항일반적으로 작동하는 것
Color and melt-flow stability during extrusion or moldingPhosphite secondary antioxidant (168) with a phenolic primary
Long-term heat aging in serviceHigh-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP)
Thin film, 섬유, low-melting compoundingLower-melting phenolic (1076) for easy dispersion
Repeated processing / 재활용 콘텐츠Raise the phosphite share in the blend and check yellowing after each pass
Humid storage or long transitHydrolysis-resistant phosphite such as 168; keep bags sealed
Food-contact articlesAsk for the grade-specific food-contact statement before trials
기존 등급 대체현재 TDS 또는 COA 보내기; 우리는 귀하가 승인한 매개변수와 일치합니다

Antioxidant Comparison

모든 열을 보려면 가로로 스와이프하거나 스크롤하세요 →

제품유형몰. 무게녹는 점Main job일반적인 시작 레벨*
SUNNOX® DLTDPThioester · secondary514.838-42°CHeat-aging synergist0.1–0.3% with a phenolic
SUNNOX® DSTDPThioester · secondary683.263–69 °CHeat-aging synergist, 낮은 변동성0.1–0.3% with a phenolic
SUNNOX® 1010Hindered phenol · primary1177.6110–125°CLong-term thermal protection0.05–0.3%
SUNNOX® 1076Hindered phenol · primary530.950–55 °CLong-term protection, easy dispersion0.05–0.3%
SUNNOX® DTDTPThioester · secondary542.9액체Heat-aging synergist, pourable0.1–0.5% with a phenolic

*시험의 출발점, 고정되지 않은 추천. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.

포장 & 저장

포장

25 PE 내부 라이너가 있는 kg 순백 또는 상자. 팔레트화; 요청 시 개인 라벨 포장.

저장

밀봉하여 서늘한 곳에 보관하세요, 마른, 열과 직사광선을 피해 통풍이 잘되는 곳. 전체 취급 세부정보는 SDS를 참조하세요..

리드타임 & 자귀

일반적으로 주문 확인 후 영업일 기준 3~15일, 수량에 따라. 본선 인도, 주요 포트에 대한 CIF 또는 DAP.

첫 번째 이메일부터 승인된 공급까지

01

Name the failure you want to prevent

Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.

02

Start from a proven blend

Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.

03

중요한 숫자를 비교하세요

For powders: 시험, melting range, volatiles and light transmittance at 425/500 nm (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.

04

공급 조건 고정

Agree packaging, monthly volume, destination port and required documents up front. 일치하는 CAS 번호만으로는 새로운 출처에 적합하지 않습니다.; run your trial and keep the approved lot COA as the reference.

귀하의 요구 사항을 알려주십시오. 우리는 등급을 일치.

Start with your polymer, 수량 및 목적지. Add your current grade or specification and we will quote against it.

정보예
중합체 / 재료PP, 체육, ABS, 화합물, 마스터배치
애플리케이션사출 성형, 압출, 영화, 섬유
현재 첨가제현재 사용하는 등급 또는 공급업체
필수사양귀하의 TDS, COA 또는 키 제한
수량평가판 주문 / 월간 간행물 / 연간 볼륨
포장기준 25 kg 또는 특정 요구 사항
목적지국가 및 항구
필요한 서류COA, SDS, 도달하다, 식품 접촉 진술서

david@sunchemgroup.com으로 이메일을 보내세요.

관련상품

SUNNOX® DSTDP

Higher-melting thioester synergist with lower volatility for long-term heat aging.

상품보기 →

SUNNOX® 1010

High-MW hindered phenolic primary antioxidant for long-term thermal protection with low volatility.

상품보기 →

SUNNOX® 1076

Low-melting hindered phenolic primary antioxidant, easy to disperse in film and compounding.

상품보기 →

SUNNOX® DTDTP

Liquid thioester synergist for ABS, PP and adhesives where a pourable additive is easier to dose.

상품보기 →

Antioxidant DLTDP FAQ

Can DLTDP be used alone?

It is not effective alone. Use it with a hindered phenolic antioxidant; ㅏ 1:1 에게 1:3 페놀성:DLTDP ratio is a common starting point.

DLTDP or DSTDP?

Both work the same way. DSTDP has a higher melting point (63–69 °C) and lower volatility; DLTDP (38-42°C) disperses more easily at low processing temperatures.

Does DLTDP affect odor or color?

Thioesters can add slight odor at high loadings and can interact with HALS in outdoor packages. Tell us the end use and we suggest the right balance.

주문하기 전에 샘플을 받을 수 있나요??

예. 폴리머를 알려주세요, 실행하려는 테스트와 필요한 수량. 샘플은 COA와 함께 배송되므로 현재 자재와 로트를 비교할 수 있습니다..

COA가 합의된 사양과 일치하지 않으면 어떻게 되나요??

합의된 사양과 차이점을 보여주는 COA를 보내주세요. (매개변수, 단위 및 시험방법). 자재를 승인하기 전에 생산 배치 기록을 통해 확인합니다., 로트가 사양을 벗어난 경우 교체하거나 다시 테스트합니다..