SUNNOX® 1135

Antioxidante 1135 Liquid Phenolic Antioxidant Supplier

SUNNOX® 1135 is a liquid hindered phenolic antioxidant. It is the standard choice for polyols and PU foam to prevent scorch, and is also used in PVC, adesivos, elastomers and lubricants.

CAS 125643-61-0 · Hindered phenol · Liquid
  • Lote COA com cada remessa
  • Amostras para seus testes
  • Suporte técnico para seu teste
Nº CAS.125643-61-0
TipoHindered phenol · Liquid
AparênciaClaro, light-yellow viscous liquid
Ensaio≥98%
DocumentosCOA / FDS / TDS

Visão geral do produto & principais benefícios

Antioxidante 1135 (C7–C9 branched alkyl ester of 3,5-di-tert-butyl-4-hydroxyphenylpropionic acid) dissolves directly in polyols, plasticizers and oils, so it is simple to meter. In flexible PU foam it protects against core discoloration (scorch) during the exothermic foaming step, usually together with an aminic or phosphite co-stabilizer.

Líquido, easy to meter

Dissolves directly in polyols, plasticizers and oils without a dispersion step.

Scorch protection

Protects flexible PU foam against core discoloration during foaming.

Low volatility for a liquid

Suitable for PVC plastisols, adhesives and elastomers.

Especificações técnicas

ParâmetroValor típico
Nome do produtoAntioxidante 1135
MarcaSUNNOX® 1135
Nº CAS.125643-61-0
Nome QuímicoBenzenepropanoic acid, 3,5-bis(1,1-dimetiletil)-4-hidroxi-, C7–C9 branched alkyl esters
AparênciaClaro, light-yellow viscous liquid
Ensaio≥98%

Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.

Applications by Polymer

Pick an application to see how 1135 is normally used and what to confirm before your trial.

Polyols & Flexible PU Foam

Added to polyol to prevent scorch in slabstock and molded foam, typically 0.1–0.5% on polyol.

Verifique antes do teste

  • Polyol type and foam grade
  • Foam density and block size
  • Current anti-scorch package
Discuta esta aplicação →

PVC & Plastisols

Liquid antioxidant for PVC compounds and plastisols.

Verifique antes do teste

  • Formulation and plasticizer
  • Temperatura de processamento
  • Color target
Discuta esta aplicação →

Adesivos, Elastômeros & Lubrificantes

Used in hot-melts, elastomers and lubricants where a liquid antioxidant is preferred.

Verifique antes do teste

  • Base polymer or oil
  • Operating temperature
  • Existing antioxidant
Discuta esta aplicação →

Seleção & comparação

Selecting an Antioxidant System

Sua necessidadeO que geralmente funciona
Color and melt-flow stability during extrusion or moldingPhosphite secondary antioxidant (168) with a phenolic primary
Long-term heat aging in serviceHigh-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP)
Thin film, fibra, low-melting compoundingLower-melting phenolic (1076) for easy dispersion
Repeated processing / conteúdo recicladoRaise the phosphite share in the blend and check yellowing after each pass
Humid storage or long transitHydrolysis-resistant phosphite such as 168; keep bags sealed
Food-contact articlesAsk for the grade-specific food-contact statement before trials
Replacing an existing gradeEnvie seu TDS ou COA atual; we match on the parameters you approve

Antioxidant Comparison

Swipe or scroll horizontally to see all columns →

ProdutoTipoMol. pesoPonto de fusãoMain jobTypical starting level*
SUNNOX® 1135Hindered phenol · liquid~390LíquidoPolyols, PU foam, PVC, adesivos0.1–0,5%
SUNNOX® 1010Hindered phenol · primary1177.6110–125 °CLong-term thermal protection0.05–0.3%
SUNNOX® 1520Fenol + thioether · liquid424.8LíquidoElastômeros, adesivos, lubrificantes0.1–0,5%
SUNNOX® 1076Hindered phenol · primary530.950–55 °CLong-term protection, easy dispersion0.05–0.3%
SUNNOX® DTDTPThioester · secondary542.9LíquidoHeat-aging synergist, pourable0.1–0.5% with a phenolic

*Starting points for trials, not fixed recommendations. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.

Embalagem & armazenar

Embalagem

Tipicamente 25 kg pails or 200 tambores de kg; IBC on request. Confirm the pack in the quotation.

Armazenar

Keep containers closed, away from heat and direct sun. Warm gently and mix before use if the liquid has thickened in cold weather. See the SDS.

Tempo de espera & terms

Typically 3–15 business days from order confirmation, depending on quantity. FOB, CIF or DAP to major ports.

Do primeiro e-mail ao fornecimento aprovado

01

Name the failure you want to prevent

Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.

02

Start from a proven blend

Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.

03

Compare os números que importam

For powders: ensaio, melting range, volatiles and light transmittance at 425/500 nm (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.

04

Bloqueie os termos de fornecimento

Agree packaging, monthly volume, destination port and required documents up front. Um número CAS correspondente por si só não qualifica uma nova fonte; run your trial and keep the approved lot COA as the reference.

Diga-nos sua necessidade. Nós combinamos a nota.

Start with your polymer, quantidade e destino. Add your current grade or specification and we will quote against it.

InformaçãoExemplo
Polymer / MaterialPP, Educação Física, abdômen, composto, lote mestre
AplicativoMoldagem por injeção, extrusão, filme, fibra
Aditivo atualClasse ou fornecedor que você usa hoje
Especificação necessáriaYour TDS, COA or key limits
QuantidadeTrial order / monthly / volume anual
EmbalagemStandard 25 kg or specific requirement
DestinoPaís e porto
Documentos necessáriosCOA, FDS, ALCANÇAR, food-contact statement

E-mail david@sunchemgroup.com

Produtos relacionados

SUNNOX® 1010

High-MW hindered phenolic primary antioxidant for long-term thermal protection with low volatility.

Ver produto →

SUNNOX® 1520

Liquid multifunctional phenolic antioxidant for elastomers, adhesives and lubricants.

Ver produto →

SUNNOX® 1076

Low-melting hindered phenolic primary antioxidant, easy to disperse in film and compounding.

Ver produto →

SUNNOX® DTDTP

Liquid thioester synergist for ABS, PP and adhesives where a pourable additive is easier to dose.

Ver produto →

Antioxidante 1135 Perguntas frequentes

Why use a liquid antioxidant in PU foam?

It dissolves directly in the polyol, so there is no dispersion step and the dose is uniform. That matters for scorch protection in large foam blocks.

What dosage is typical?

0.1–0.5% on polyol is a common range, depending on foam density and block size. Confirm in your foam trial.

Which COA parameters matter?

Ensaio, color and viscosity. Tell us your incoming limits and we quote against them.

Posso obter uma amostra antes de fazer o pedido?

Sim. Diga-nos o polímero, o teste que você planeja realizar e a quantidade necessária. As amostras são enviadas com um COA para que você possa comparar o lote com o material atual.

E se um COA não corresponder à especificação acordada?

Envie-nos a especificação acordada e o COA mostrando a diferença (parâmetro, unidade e método de teste). Verificamos com o registro do lote de produção antes de você aceitar o material, e substitua ou teste novamente quando o lote estiver fora das especificações.

Discuss your Antioxidant 1135 requisitos

Contato
lupa