SUNSORB® 328 (UV-328) is a benzotriazole UV absorber used in coatings and plastics. UV-328 is listed under the Stockholm Convention and as a REACH SVHC, so its use is restricted in many markets; check your destination first.
UV-328 (2-(2H-benzotriazol-2-il)-4,6-di-tert-pentylphenol) has been used in automotive coatings, PVC and polyolefins. It is now listed for elimination under the Stockholm Convention (with limited exemptions) and is a REACH SVHC. We supply it only where the destination allows, and help buyers move to alternatives such as 329, 234 ou líquido 384-2 for coatings.
We check your destination and end use before quoting.
We propose and supply alternatives for restricted markets.
Historically used in coatings, PVC and polyolefins.
| Parâmetro | Valor típico |
|---|---|
| Nome do produto | UV Absorber UV-328 |
| Marca | SUNSORB® 328 |
| Nº CAS. | 25973-55-1 |
| Nome Químico | 2-(2H-Benzotriazol-2-il)-4,6-di-tert-pentylphenol |
| Fórmula Molecular | C22H29N3O |
| Peso molecular | 351.5 |
| Aparência | Light-yellow powder |
| Ponto de fusão | 80–83 °C |
| Ensaio | ≥99% |
Especificação típica. Cada remessa é fornecida com um COA de lote; os limites que se aplicam ao seu pedido estão confirmados na cotação e no contrato.
Escolha um aplicativo para ver como 328 é normalmente usado e o que confirmar antes do teste.
Listed under the Stockholm Convention and REACH. Use depends on country and on specific exemptions.
For coatings, líquido 384-2 or triazine 400 with a liquid HALS are common replacements.
For plastics, 329 ou 234 are common replacements depending on processing temperature.
| Sua necessidade | O que geralmente funciona |
|---|---|
| Clear or light-colored polyolefin parts and film | Benzophenone (531) or benzotriazole (326) at low loading |
| High processing temperature (computador, BICHO DE ESTIMAÇÃO, PA) | Low-volatility grades: 234, 360 or 1577-type triazines |
| Thin films and fibers | Higher-MW, low-volatility grades so the absorber is not lost in processing |
| Solvent-borne and waterborne coatings | Liquid benzotriazoles (384-2, 1130) or triazine (400), paired with a HALS |
| Outdoor service longer than one season | UV absorber plus a HALS; the absorber filters, the HALS stops radical chains |
| Exports to the EU | Check REACH status first; some benzotriazoles (327, 328) are restricted |
| Substituindo uma nota existente | Envie seu TDS ou COA atual; we match on chemistry and the parameters you approve |
Deslize ou role horizontalmente para ver todas as colunas →
| Produto | Chemistry | Mol. peso | Ponto de fusão / form | Melhor ajuste | Nível inicial típico* |
|---|---|---|---|---|---|
| SUNSORB® 328 | Benzotriazol | 351.5 | 80–83 °C | Revestimentos, PVC (restricted markets) | 0.1–0,5% |
| SUNSORB® 329 | Benzotriazol | 323.4 | 103–105 °C | computador, BICHO DE ESTIMAÇÃO, PVC, PMMA | 0.1–0,5% |
| SUNSORB® 234 | Benzotriazol | 447.6 | 137–141ºC | computador, BICHO DE ESTIMAÇÃO, PA at high temperature | 0.1–0,5% |
| SUNSORB® 384-2 | Benzotriazol, líquido | - | Líquido | Revestimentos | 1–3% on binder solids |
| SUNSORB® 400 | Hydroxyphenyl-triazine, líquido | - | Líquido | Revestimentos automotivos e industriais | 1–3% on binder solids |
*Pontos de partida para testes, recomendações não fixas. Loading depends on part thickness, pigment, target service life and the HALS used alongside. UV absorbers and HALS work by different mechanisms and are usually combined.
25 sacos líquidos ou caixas de kg com forro interno de PE. Paletizado; embalagem de marca própria mediante solicitação.
Mantenha selado em local fresco, seco, local ventilado, longe do calor e do sol direto. Consulte a FDS para obter detalhes completos de manuseio.
Normalmente de 3 a 15 dias úteis a partir da confirmação do pedido, dependendo da quantidade. FOB, CIF ou DAP para os principais portos.
Indoor light behind glass, outdoor temperate climate and desert or tropical exposure need very different packages. Note the target service life and the weathering test you use (xenon or QUV, horas, ΔE or gloss retention).
A UV absorber works by filtering, so it needs enough path length: thick parts need less, thin films and fibers need more and need a low-volatility grade. Check the absorber survives your processing temperature.
For outdoor use the standard approach is UV absorber plus HALS. Send your current package and pigment system and we suggest a starting combination for the trial.
Some benzotriazoles are restricted in the EU and other markets. Tell us the destination and end use, and we confirm the REACH and food-contact position of the grade before you order.
Comece com seu material, espessura da peça, quantidade e destino. Add your current UV package and we will quote against it.
| Informação | Exemplo |
|---|---|
| Polímero / Material | PP, Educação Física, abdômen, composto, lote mestre |
| Aplicativo | Moldagem por injeção, extrusão, filme, fibra |
| Aditivo atual | Classe ou fornecedor que você usa hoje |
| Especificação necessária | Seu TDS, COA ou limites principais |
| Quantidade | Pedido de teste / mensal / volume anual |
| Embalagem | Padrão 25 kg ou exigência específica |
| Destino | País e porto |
| Documentos necessários | COA, FDS, ALCANÇAR, declaração de contato com alimentos |
Hydroxyphenyl-triazine liquid UV absorber for durable automotive and industrial coatings.
Ver produto →It is listed under the Stockholm Convention for elimination, with limited exemptions, and is a REACH SVHC. Rules differ by country, so tell us your market before ordering.
Liquid benzotriazole 384-2 or hydroxyphenyl-triazine 400, combined with a liquid HALS such as 292, are common replacements.
329 ou 234, depending on polymer and processing temperature. Re-run your weathering test after switching.
Sim. Diga-nos o polímero, o teste que você planeja realizar e a quantidade necessária. As amostras são enviadas com um COA para que você possa comparar o lote com o material atual.
Envie-nos a especificação acordada e o COA mostrando a diferença (parâmetro, unidade e método de teste). Verificamos com o registro do lote de produção antes de você aceitar o material, e substitua ou teste novamente quando o lote estiver fora das especificações.