Long-lasting protection
The regenerative HALS mechanism gives long protection; set the loading in your own weathering trial.
LUMIÈRE DU SOLEIL® 770 is a low-molecular-weight hindered amine light stabilizer (HALS) pour polyoléfines, cross-linked polyethylene and olefin copolymers. It is often used together with a UV absorber, an antioxidant or a polymeric HALS.
HALS 770 (bis(2,2,6,6-tétraméthyl-4-pipéridyle) sébacé) traps the free radicals formed by UV exposure and regenerates, so it protects for a long time at low loading. Its low molecular weight (480.7) lets it move to the part surface quickly, which suits thick parts; for thin film and fiber it is often blended with a polymeric HALS such as 944.
The regenerative HALS mechanism gives long protection; set the loading in your own weathering trial.
Fast migration to the surface suits thick moldings.
The TDS notes synergy with antioxidants and UV absorbers; it is often combined with 944 for longer life.
| Paramètre | Valeur typique |
|---|---|
| Nom du produit | Stabilisateur de lumière 770 |
| Marque | LUMIÈRE DU SOLEIL® 770 |
| Numéro CAS. | 52829-07-9 |
| Nom chimique | Bis(2,2,6,6-tétraméthyl-4-pipéridyle) sébacé |
| Formule moléculaire | C28H52N2O4 |
| Masse moléculaire | 480.7 |
| Apparence | Solide blanc |
| Point de fusion | 81.0–86.0 °C |
| Loss on Drying | ≤0.50% |
| Light Transmittance, 425 nm | ≥98,0 % |
| Light Transmittance, 500 nm | ≥99,0 % |
| Cendre | ≤0.10% |
| Pureté | ≥99,0 % |
| Couleur | ≤25 APHA |
Standard values from the SUNLIGHT® 770 DT (V6.2). Chaque envoi est fourni avec un COA de lot; les limites applicables à votre commande sont confirmées dans le devis et le contrat.
The TDS lists polyolefins, cross-linked polyethylene and olefin copolymers. Pick a group to see what to confirm before your trial.
Listed in the TDS for polyolefin materials, especially thicker parts where a low-molecular-weight HALS reaches the surface quickly.
Listed in the TDS for cross-linked polyethylene. Share the cross-linking method and other additives.
Listed in the TDS for olefin copolymers, usually alongside an antioxidant and a UV absorber.
| Votre exigence | Ce qui fonctionne habituellement |
|---|---|
| Thick PP and PE parts | Low-MW HALS (770) for fast migration to the surface |
| Films minces, tapes and fibers | Polymeric HALS (944, 622) for low volatility and extraction resistance |
| Agricultural film exposed to pesticides | Polymeric HALS with good resistance to acidic residues; ask about the specific chemicals |
| Automotive and industrial coatings | Liquid HALS (292) with a UV absorber |
| Acid-catalyzed coatings | Non-basic NOR-type HALS (123) |
| Long outdoor life | HALS plus UV absorber, often a blend of a low-MW and a polymeric HALS |
| Remplacement d'une note existante | Envoyez votre TDS ou COA actuel; we match on the parameters you approve |
Faites glisser ou faites défiler horizontalement pour voir toutes les colonnes →
| Produit | Taper | Meilleur ajustement |
|---|---|---|
| LUMIÈRE DU SOLEIL® 770 | HALS monomères | Thick polyolefin parts |
| LUMIÈRE DU SOLEIL® 944 | Polymeric HALS | PP/PE film, tape, fibre |
| LUMIÈRE DU SOLEIL® 622 | Polymeric HALS | PE film, PP fiber |
| SUNSORB® 326 | Benzotriazole UV absorber | Used with HALS in polyolefins |
| SUNSORB® 531 | Benzophenone UV absorber | Used with HALS in PE and PP |
Combining a HALS with a UV absorber is usual for outdoor use. Définissez les niveaux dans votre propre essai.
25 kg cartons with a plastic inner bag, or packed to customer requirement.
Keep the container tightly closed in a dry, well-ventilated place. Voir la FDS pour plus de détails sur la manipulation.
Les qualités régulières sont généralement en stock. Pour les gros volumes, le délai est confirmé dans le devis. Nous citons FOB et CIF.
Note the climate, the expected service life and your weathering test (xenon or QUV hours, retained elongation, gloss or ΔE). For agricultural film, list the pesticides and fumigants the film will meet.
Low-MW HALS move to the surface quickly and suit thick parts; polymeric HALS resist loss from thin films and fibers. Many outdoor packages blend both.
HALS are basic and can interact with acidic additives, halogenated flame retardants, some pigments and sulfur-containing antioxidants. Send your full formulation so we can flag conflicts before the trial.
Agree physical form (powder or granule), conditionnement, monthly volume and documents up front. A matching CAS number alone does not qualify a new source; run your weathering test and keep the approved lot COA as the reference.
Commencez par votre matériel, épaisseur de la pièce, quantité et destination. Add your current stabilizer package and we will quote against it.
| Information | Exemple |
|---|---|
| Polymère / Matériel | PP, PE, abdos, composé, mélange maître |
| Application | Moulage par injection, extrusion, film, fibre |
| Additif actuel | Qualité ou fournisseur que vous utilisez aujourd'hui |
| Spécification requise | Votre TDS, COA ou limites clés |
| Quantité | Commande à l'essai / mensuel / volume annuel |
| Emballage | Standard 25 kg ou exigence spécifique |
| Destination | Pays et port |
| Documents nécessaires | COA, FDS, ATTEINDRE, déclaration de contact alimentaire |
Polymeric HALS for PP and PE film, tape and fiber with low volatility.
Voir le produit →Polymeric HALS with low basicity, used in PE film and PP fiber.
Voir le produit →Absorbeur UV de benzotriazole chloré pour polyoléfines, PVC et adhésifs.
Voir le produit →Benzophenone UV absorber for polyolefins and PVC, cost-effective and widely used.
Voir le produit →770 is best for thick parts; 944 (polymeric) is better for thin film and fiber. Many outdoor packages blend both.
Le niveau dépend de votre polymère, épaisseur de la pièce, autres additifs et conditions d'essai, alors mets-le dans ton propre essai. La TDS est disponible sur demande.
Low-MW HALS can be lost from thin film; polymeric HALS such as 944 ou 622 are usually preferred there.
Oui. Parlez-nous du polymère, le test que vous prévoyez d'effectuer et la quantité dont vous avez besoin. Les échantillons sont expédiés avec un COA afin que vous puissiez comparer le lot avec votre matériel actuel.
Envoyez-nous la spécification convenue et le COA montrant la différence (paramètre, unité et méthode de test). Nous le vérifions avec le dossier de lot de production avant d'accepter le matériel, et remplacer ou tester à nouveau lorsque le lot est hors spécifications.