Low basicity
Fewer interactions with acidic additives and pigments.
LUMIÈRE DU SOLEIL® 622 is a polymeric HALS with low basicity and very low volatility. It is used in PE film, PP fiber and other thin polyolefin articles, including applications with food-contact requirements.
HALS 622 (butanedioic acid, ester diméthylique, polymer with 4-hydroxy-2,2,6,6-tetramethyl-1-piperidineethanol) has a number-average molecular weight of about 3100–4000. Its low basicity reduces interaction with acidic components and pigments, and its high molecular weight resists loss from thin sections.
Fewer interactions with acidic additives and pigments.
Low volatility and extraction for film and fiber.
Widely used where food-contact compliance is needed; ask for the statement.
| Paramètre | Valeur typique |
|---|---|
| Nom du produit | Stabilisateur de lumière 622 |
| Marque | LUMIÈRE DU SOLEIL® 622 |
| Numéro CAS. | 65447-77-0 |
| Masse moléculaire | Mn 3100–4000 |
| Apparence | White to light-yellow powder or granule |
| Melting Range | 50–70 °C |
| Cendre | ≤0,1% |
| Matière volatile | ≤0,5% |
Spécification typique. Chaque envoi est fourni avec un COA de lot; les limites applicables à votre commande sont confirmées dans le devis et le contrat.
Choisissez une application pour voir comment 622 est normalement utilisé et que confirmer avant votre essai.
UV stabilizer for PE film.
Used in PP fiber and tape for outdoor use.
Also used in EVA, PU and adhesives.
| Votre exigence | Ce qui fonctionne habituellement |
|---|---|
| Thick PP and PE parts | Low-MW HALS (770) for fast migration to the surface |
| Films minces, tapes and fibers | Polymeric HALS (944, 622) for low volatility and extraction resistance |
| Agricultural film exposed to pesticides | Polymeric HALS with good resistance to acidic residues; ask about the specific chemicals |
| Automotive and industrial coatings | Liquid HALS (292) with a UV absorber |
| Acid-catalyzed coatings | Non-basic NOR-type HALS (123) |
| Long outdoor life | HALS plus UV absorber, often a blend of a low-MW and a polymeric HALS |
| Remplacement d'une note existante | Envoyez votre TDS ou COA actuel; we match on the parameters you approve |
Faites glisser ou faites défiler horizontalement pour voir toutes les colonnes →
| Produit | Taper | Mol. poids | Formulaire | Meilleur ajustement |
|---|---|---|---|---|
| LUMIÈRE DU SOLEIL® 622 | Polymeric HALS | Mn 3100–4000 | Powder or granule | PE film, PP fiber |
| LUMIÈRE DU SOLEIL® 944 | Polymeric HALS | Mn 2000–3100 | Granule or powder | PP/PE film, tape, fibre |
| LUMIÈRE DU SOLEIL® 770 | HALS monomères | 480.7 | Poudre ou granule blanc | PP épais, PE, styréniques |
| LUMIÈRE DU SOLEIL® 119 | High-MW HALS | 2286 | Poudre ou granule blanc | Thin PP/PE articles, long outdoor life |
| SUNSORB® 531 | Benzophénone | 326.4 | 47–49 °C | PE, PP, PVC |
Définissez les niveaux dans votre propre essai. The right level depends on part thickness, pigments, charges, agrochemical exposure and target service life. Combining a HALS with a UV absorber is usual for outdoor use.
25 Sacs nets de 1 kg ou cartons avec doublure intérieure en PE. Palettisé.
Conserver scellé au frais, sec, endroit aéré à l'abri de la chaleur et du soleil direct. Voir la FDS pour plus de détails sur la manipulation.
Les qualités régulières sont généralement en stock. Pour les gros volumes, le délai est confirmé dans le devis. Nous citons FOB et CIF.
Note the climate, the expected service life and your weathering test (xenon or QUV hours, retained elongation, gloss or ΔE). For agricultural film, list the pesticides and fumigants the film will meet.
Low-MW HALS move to the surface quickly and suit thick parts; polymeric HALS resist loss from thin films and fibers. Many outdoor packages blend both.
HALS are basic and can interact with acidic additives, halogenated flame retardants, some pigments and sulfur-containing antioxidants. Send your full formulation so we can flag conflicts before the trial.
Agree physical form (powder or granule), conditionnement, monthly volume and documents up front. A matching CAS number alone does not qualify a new source; run your weathering test and keep the approved lot COA as the reference.
Commencez par votre matériel, épaisseur de la pièce, quantité et destination. Add your current stabilizer package and we will quote against it.
| Information | Exemple |
|---|---|
| Polymère / Matériel | PP, PE, abdos, composé, mélange maître |
| Application | Moulage par injection, extrusion, film, fibre |
| Additif actuel | Qualité ou fournisseur que vous utilisez aujourd'hui |
| Spécification requise | Votre TDS, COA ou limites clés |
| Quantité | Commande à l'essai / mensuel / volume annuel |
| Emballage | Standard 25 kg ou exigence spécifique |
| Destination | Pays et port |
| Documents nécessaires | COA, FDS, ATTEINDRE, déclaration de contact alimentaire |
Polymeric HALS for PP and PE film, tape and fiber with low volatility.
Voir le produit →HALS à faible poids moléculaire pour les pièces épaisses en polyoléfine et en styrène.
Voir le produit →High-MW HALS for thin PP and PE articles needing long outdoor life.
Voir le produit →Benzophenone UV absorber for polyolefins and PVC, cost-effective and widely used.
Voir le produit →Lower basicity and food-contact use. 944 generally gives higher UV performance per unit.
Le niveau dépend de votre polymère, épaisseur de la pièce, autres additifs et conditions d'essai, alors mets-le dans ton propre essai. La TDS est disponible sur demande.
Oui, blends with 944 ou 770 are common in outdoor polyolefins.
Oui. Parlez-nous du polymère, le test que vous prévoyez d'effectuer et la quantité dont vous avez besoin. Les échantillons sont expédiés avec un COA afin que vous puissiez comparer le lot avec votre matériel actuel.
Envoyez-nous la spécification convenue et le COA montrant la différence (paramètre, unité et méthode de test). Nous le vérifions avec le dossier de lot de production avant d'accepter le matériel, et remplacer ou tester à nouveau lorsque le lot est hors spécifications.