DLTDP Thioester Antioxidant Supplier

SUNNOX® DLTDP (dilauryl thiodipropionate) is a thioester secondary antioxidant. Used with a phenolic primary such as 1010 или же 1076, it markedly extends long-term heat aging in polyolefins, ABS and rubber.

КАС 123-28-4 · Thioester · Secondary antioxidant
Illustration of polymer pellets, molded samples and film
Application illustration — not a photograph of the product

Обзор продукта

DLTDP decomposes hydroperoxides into stable products, so it removes the fuel for continued oxidation during long service at elevated temperature. On its own it is a weak antioxidant; combined with a hindered phenol it gives a strong synergy for heat-aging performance. Typical blends run at 1:1 к 1:3 фенольный:DLTDP.

Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.

Key Benefits

Long-term heat aging

Synergy with phenolic antioxidants extends oven-aging life well beyond the phenolic alone.

Low melting point

Melts at 38–42 °C and disperses easily in compounding and masterbatch.

Cost-effective boost

Often lets you hold or reduce the phenolic level for the same heat-aging target.

Технические характеристики

Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.

ParameterTypical value
Название продуктаАнтиоксидант ДЛТДП
БрендSUNNOX® DLTDP
Номер КАС.123-28-4
Химическое названиеDilauryl 3,3'-thiodipropionate
Молекулярная формулаC30H58O4S
Молекулярный вес514.8
видWhite crystalline powder or flake
Температура плавления38–42 °C
Acid Value≤0.05 mg KOH/g
Volatile Matter≤0.05%

Applications by Polymer

Pick an application to see how DLTDP is normally used and what to confirm before your trial.

Illustration of polymer film, molded components and masterbatch granules
Polymer application illustration

Полиолефины

Used with 1010 или же 1076 in PP and PE parts that must pass long oven-aging tests, such as appliance and automotive components.

What to confirm for your application

  • Heat-aging test (температура, часы)
  • Phenolic antioxidant and its level
  • Odor requirements for the part
Discuss this application →

АБС & Styrenics

Improves heat-aging of ABS and HIPS together with a phenolic antioxidant.

What to confirm for your application

  • Grade and other additives
  • Service temperature
  • Color target
Discuss this application →

Резина, Клеи & Смазочные материалы

Used in rubber, hot-melts and lubricants as a heat-aging synergist.

What to confirm for your application

  • Base polymer or oil
  • Operating temperature
  • Existing antioxidant package
Discuss this application →

Упаковка & Storage

Упаковка

25 kg net bags or cartons with a PE inner liner. Palletized; private-label packing on request.

Storage

Keep sealed in a cool, сухой, ventilated place away from heat and direct sun. See the SDS for full handling details.

Время выполнения & terms

Typically 3–15 business days from order confirmation, depending on quantity. ФОБ, CIF or DAP to major ports.

Technical & Buying Information

Selecting an Antioxidant System

Your requirementWhat usually works
Color and melt-flow stability during extrusion or moldingPhosphite secondary antioxidant (168) with a phenolic primary
Long-term heat aging in serviceHigh-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP)
Thin film, волокно, low-melting compoundingLower-melting phenolic (1076) for easy dispersion
Repeated processing / переработанный контентRaise the phosphite share in the blend and check yellowing after each pass
Humid storage or long transitHydrolysis-resistant phosphite such as 168; keep bags sealed
Food-contact articlesAsk for the grade-specific food-contact statement before trials
Replacing an existing gradeSend your current TDS or COA; we match on the parameters you approve

Antioxidant Comparison

Swipe or scroll horizontally to see all columns →

ПродуктТипMol. weightТемпература плавленияMain jobTypical starting level*
SUNNOX® DLTDPThioester · secondary514.838–42 °CHeat-aging synergist0.1–0.3% with a phenolic
СУННОКС® ДСТДПThioester · secondary683.263–69 °CHeat-aging synergist, более низкая волатильность0.1–0.3% with a phenolic
САННОКС® 1010Hindered phenol · primary1177.6110–125 °CLong-term thermal protection0.05–0.3%
САННОКС® 1076Hindered phenol · primary530.950–55 °CLong-term protection, easy dispersion0.05–0.3%
СУННОКС® ДТДТПThioester · secondary542.9ЖидкостьHeat-aging synergist, pourable0.1–0.5% with a phenolic

*Starting points for trials, not fixed recommendations. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.

Документы & Качественный

Сертификат подлинности — Сертификат анализа

Issued for every batch shipped, with the test results for that lot.

TDS — Технический паспорт

Typical properties and specification for evaluation and supplier approval.

SDS — Safety Data Sheet

GHS-format handling, storage and transport information.

Образцы

Lab samples for evaluation; tell us the test you plan to run so the sample size fits.

Third-party testing

SGS or Intertek testing can be arranged on request.

Regulatory statements

ДОСТИГАТЬ, food-contact and other statements are issued per grade and destination; ask before ordering.

Antioxidant DLTDP Buyer Guide

Name the failure you want to prevent

Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.

Start from a proven blend

Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.

Compare the numbers that matter

For powders: анализ, melting range, volatiles and light transmittance at 425/500 нм (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.

Lock in supply terms

Agree packaging, monthly volume, destination port and required documents up front. A matching CAS number alone does not qualify a new source; run your trial and keep the approved lot COA as the reference.

Request a Quotation for Antioxidant DLTDP

Start with your polymer, количество и назначение. Add your current grade or specification and we will quote against it.

InformationExample
Polymer / MaterialПП, ЧП, АБС, сложный, маточная смесь
ПриложениеInjection molding, экструзия, фильм, волокно
Current additiveGrade or supplier you use today
Required specificationYour TDS, COA or key limits
QuantityTrial order / monthly / annual volume
УпаковкаStandard 25 kg or specific requirement
DestinationCountry and port
Documents neededсертификат подлинности, паспорт безопасности, ДОСТИГАТЬ, food-contact statement
Send RFQ by EmailContact SUNCHEM →

Related Antioxidants

СУННОКС® ДСТДП

Higher-melting thioester synergist with lower volatility for long-term heat aging.

View product →

САННОКС® 1010

High-MW hindered phenolic primary antioxidant for long-term thermal protection with low volatility.

View product →

САННОКС® 1076

Low-melting hindered phenolic primary antioxidant, easy to disperse in film and compounding.

View product →

СУННОКС® ДТДТП

Liquid thioester synergist for ABS, PP and adhesives where a pourable additive is easier to dose.

View product →

Antioxidant DLTDP FAQ

Can DLTDP be used alone?

It is not effective alone. Use it with a hindered phenolic antioxidant; а 1:1 к 1:3 фенольный:DLTDP ratio is a common starting point.

DLTDP or DSTDP?

Both work the same way. DSTDP has a higher melting point (63–69 °C) and lower volatility; DLTDP (38–42 °C) disperses more easily at low processing temperatures.

Does DLTDP affect odor or color?

Thioesters can add slight odor at high loadings and can interact with HALS in outdoor packages. Tell us the end use and we suggest the right balance.

Can I get a sample before ordering?

Да. Tell us the polymer, the test you plan to run and the quantity you need. Samples ship with a COA so you can compare the lot against your current material.

What if a COA does not match our agreed specification?

Send us the agreed specification and the COA showing the difference (parameter, unit and test method). We check it with the production batch record before you accept the material, and replace or re-test where the lot is out of specification.

Discuss Your Antioxidant DLTDP Requirements

Send your application, specification and quantity to request a quotation or supporting documents.

лупа