Long-term heat protection
Keeps tensile and impact properties through long service at elevated temperature, the main reason 1010 is the default phenolic in polyolefins.
SUNNOX® 1010 is a high-molecular-weight hindered phenolic primary antioxidant. It gives long-term thermal protection with very low volatility and extraction, in polyolefins, engineering plastics, rubber and adhesives.
Antioxidant 1010 traps the free radicals that drive thermal oxidation, so plastics keep their strength and appearance through years of service at elevated temperature. Its molecular weight of 1177.6 keeps it in the polymer: it does not evaporate during processing and resists extraction by water and solvents. For processing stability it is normally blended with a phosphite such as 168, and with a thioester (DLTDP / DSTDP) where long-term heat aging is critical.
Keeps tensile and impact properties through long service at elevated temperature, the main reason 1010 is the default phenolic in polyolefins.
High molecular weight means low volatility in processing and low migration or extraction in use.
Used in PE, PP, POM, ABS, PS, PVC, PA, PET, PU, rubber, hot-melt adhesives and lubricants. Odorless and non-staining.
| Parameter | Typical value |
|---|---|
| Product Name | Antioxidant 1010 |
| Brand | SUNNOX® 1010 |
| CAS No. | 6683-19-8 |
| Chemical Name | Pentaerythritol tetrakis[3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate] |
| Molecular Formula | C73H108O12 |
| Molecular Weight | 1177.6 |
| Appearance | White crystalline powder |
| Melting Point | 110–125 °C |
| Effective Content | ≥98.0% |
| Main Component | ≥94.0% |
| Ash | ≤0.1% |
| Volatile Matter | ≤0.5% |
| Light Transmittance — 425 nm | ≥96% |
| Light Transmittance — 500 nm | ≥98% |
| Solubility (20 °C, w/w) | Chloroform 71%, dichloromethane 63%, benzene 55%, ethyl acetate 47%, acetone 46%, methanol 0.9%, hexane 0.3%, water <0.01% |
Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.
Pick a material family to see how 1010 is normally used and what to confirm before your trial.
The default long-term antioxidant for PP and PE pipe, film, fiber and molded parts. Typically 0.05–0.3%, blended with 168 (1:1 or 1:2 1010:168) for processing stability.
Used for heat-aging protection in POM, PA, PET/PBT, ABS and PS, often at the higher end of the dosage range for parts exposed to heat.
Protects SBS, SIS, EPDM and EVA-based hot-melts and adhesives from oxidation during melting and storage, without staining.
Used as a co-antioxidant in PVC and PU systems and as a high-temperature antioxidant in lubricants and oils.
| Your requirement | What usually works |
|---|---|
| Color and melt-flow stability during extrusion or molding | Phosphite secondary antioxidant (168) with a phenolic primary |
| Long-term heat aging in service | High-MW phenolic primary (1010), often with a thioester (DLTDP / DSTDP) |
| Thin film, fiber, low-melting compounding | Lower-melting phenolic (1076) for easy dispersion |
| Repeated processing / recycled content | Raise the phosphite share in the blend and check yellowing after each pass |
| Humid storage or long transit | Hydrolysis-resistant phosphite such as 168; keep bags sealed |
| Food-contact articles | Ask for the grade-specific food-contact statement before trials |
| Replacing an existing grade | Send your current TDS or COA; we match on the parameters you approve |
Swipe or scroll horizontally to see all columns →
| Product | Type | Mol. weight | Melting point | Main job | Typical starting level* |
|---|---|---|---|---|---|
| SUNNOX® 1010 | Hindered phenol · primary | 1177.6 | 110–125 °C | Long-term thermal protection | 0.05–0.3% |
| SUNNOX® 168 | Phosphite · secondary | 646.9 | 183–187 °C | Processing stability, color | 0.05–0.2% with a phenolic |
| SUNNOX® 1076 | Hindered phenol · primary | 530.9 | 50–55 °C | Long-term protection, easy dispersion | 0.05–0.3% |
| SUNNOX® DLTDP | Thioester · secondary | 514.8 | 38–42 °C | Heat-aging synergist | 0.1–0.3% with a phenolic |
| SUNNOX® DSTDP | Thioester · secondary | 683.2 | 63–69 °C | Heat-aging synergist, lower volatility | 0.1–0.3% with a phenolic |
*Starting points for trials, not fixed recommendations. The right level depends on resin, catalyst residue, processing temperature and service life. Primary and secondary antioxidants do different jobs and are not interchangeable.
25 kg net in a plastic inner bag inside a paperboard drum or carton. Private-label packing on request.
Stable under normal conditions. Keep sealed, away from heat and moisture. See the SDS for full handling details.
Typically 3–15 business days from order confirmation, depending on quantity. FOB, CIF or DAP to major ports.
Yellowing or melt-flow change during processing points to the phosphite share; embrittlement or cracking after months in service points to the phenolic and thioester share. Note recycled content and the number of extrusion passes.
Most polyolefin packages start from a phenolic primary plus a phosphite secondary, then adjust. Send your current package and we suggest a starting blend for the trial instead of changing several variables at once.
For powders: assay, melting range, volatiles and light transmittance at 425/500 nm (a direct read on color). Ask for the same parameters on our COA that appear on your incoming-inspection sheet.
Agree packaging, monthly volume, destination port and required documents up front. A matching CAS number alone does not qualify a new source; run your trial and keep the approved lot COA as the reference.
Start with your polymer, quantity and destination. Add your current grade or specification and we will quote against it.
| Information | Example |
|---|---|
| Polymer / Material | PP, PE, ABS, compound, masterbatch |
| Application | Injection molding, extrusion, film, fiber |
| Current additive | Grade or supplier you use today |
| Required specification | Your TDS, COA or key limits |
| Quantity | Trial order / monthly / annual volume |
| Packaging | Standard 25 kg or specific requirement |
| Destination | Country and port |
| Documents needed | COA, SDS, REACH, food-contact statement |
Hydrolysis-resistant phosphite secondary antioxidant for color and melt-flow protection during processing.
View product →Low-melting hindered phenolic primary antioxidant, easy to disperse in film and compounding.
View product →Thioester secondary antioxidant that boosts long-term heat aging when used with a phenolic.
View product →Higher-melting thioester synergist with lower volatility for long-term heat aging.
View product →Both are hindered phenolic primaries. 1010 (MW 1177.6) has lower volatility and extraction, so it is preferred for long service life and high-temperature use. 1076 (MW 530.9, melts at 50–55 °C) disperses more easily in film and low-temperature compounding.
0.05–0.3% in most polyolefins, higher for parts that must pass long heat-aging tests. Use it with 168 for processing stability. Confirm the level in your own heat-aging trial.
1010 is widely used in food-contact polymers. Ask us for the grade-specific food-contact statement for your market before you start trials.
Yes. Tell us the polymer, the test you plan to run and the quantity you need. Samples ship with a COA so you can compare the lot against your current material.
Send us the agreed specification and the COA showing the difference (parameter, unit and test method). We check it with the production batch record before you accept the material, and replace or re-test where the lot is out of specification.