Gloss retention
Prevents surface cracking and gloss loss.
LUMIÈRE DU SOLEIL® 292 is a liquid hindered amine light stabilizer for automotive, industrial and wood coatings. Used with a UV absorber such as 384-2 ou 1130, it prevents cracking and gloss loss.

HALS 292 is a mixture of bis(1,2,2,6,6-pentamethyl-4-piperidyl) sebacate and methyl 1,2,2,6,6-pentamethyl-4-piperidyl sebacate, supplied as a liquid that blends easily into coatings. It traps radicals at the coating surface, preserving gloss and preventing cracking, and works best with a UV absorber that protects the deeper layers and the substrate.
Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.
Prevents surface cracking and gloss loss.
Blends directly into coatings.
Standard partner for 384-2, 1130 et 400.
Typical specification. Every shipment is supplied with a batch COA; the limits that apply to your order are confirmed in the quotation and contract.
| Parameter | Typical value |
|---|---|
| Nom du produit | Stabilisateur de lumière 292 |
| Marque | LUMIÈRE DU SOLEIL® 292 |
| Numéro CAS. | 41556-26-7 / 82919-37-7 |
| Composition | Bis(1,2,2,6,6-pentamethyl-4-piperidyl) sébacé + methyl 1,2,2,6,6-pentamethyl-4-piperidyl sebacate |
| Apparence | Light-yellow liquid |
Pick an application to see how 292 is normally used and what to confirm before your trial.

Typically 0.5–2% on binder solids with a UV absorber.
Protects exterior wood coatings against cracking and gloss loss.
Basic HALS can interfere with acid catalysts; for these systems use non-basic 123 plutôt.
Typiquement 25 kg pails or 200 fûts de kg; IBC on request. Confirm the pack in the quotation.
Keep containers closed, away from heat and direct sun. Warm gently and mix before use if the liquid has thickened in cold weather. See the SDS.
Typically 3–15 business days from order confirmation, depending on quantity. GOUSSET, CIF or DAP to major ports.
Note the climate, the expected service life and your weathering test (xenon or QUV hours, retained elongation, gloss or ΔE). For agricultural film, list the pesticides and fumigants the film will meet.
Low-MW HALS move to the surface quickly and suit thick parts; polymeric HALS resist loss from thin films and fibers. Many outdoor packages blend both.
HALS are basic and can interact with acidic additives, halogenated flame retardants, some pigments and sulfur-containing antioxidants. Send your full formulation so we can flag conflicts before the trial.
Agree physical form (powder or granule), conditionnement, monthly volume and documents up front. A matching CAS number alone does not qualify a new source; run your weathering test and keep the approved lot COA as the reference.
Start with your material, part thickness, quantité et destination. Add your current stabilizer package and we will quote against it.
| Information | Example |
|---|---|
| Polymer / Material | PP, PE, abdos, composé, mélange maître |
| Application | Injection molding, extrusion, film, fibre |
| Current additive | Grade or supplier you use today |
| Required specification | Your TDS, COA or key limits |
| Quantity | Trial order / monthly / annual volume |
| Emballage | Standard 25 kg or specific requirement |
| Destination | Country and port |
| Documents needed | COA, FDS, ATTEINDRE, food-contact statement |
Liquid benzotriazole UV absorber for coatings, often paired with liquid HALS.
View product →Hydroxyphenyl-triazine liquid UV absorber for durable automotive and industrial coatings.
View product →It can interfere with acid catalysts. For acid-cure systems, the non-basic NOR HALS 123 is the usual choice.
0.5–2% on binder solids, with 1–3% of a UV absorber.
It is mainly for coatings; for plastics, solid HALS such as 770 ou 944 are used.
Oui. Tell us the polymer, the test you plan to run and the quantity you need. Samples ship with a COA so you can compare the lot against your current material.
Send us the agreed specification and the COA showing the difference (parameter, unit and test method). We check it with the production batch record before you accept the material, and replace or re-test where the lot is out of specification.
Send your application, specification and quantity to request a quotation or supporting documents.